Thinky applications
Applications | THINKY Mixer | VIscosity, Density, Particle Volume or Size |
Datasheet | ||
1 | Ceramic (10 V%) | Dispersion Defoaming | ARE-250 2 minutes | Barium Titanate – 6.02g/cm3 Micron particle, 10 volume %, (Total 120g) | View |
2 | Nano Ceramic (70 V%) | Dispersion Defoaming | ARE-250 3 minutes | Aluminum oxide – 0.5µm Nano particle, 3.97g/cm3 50-70 volume % | View |
3 | 2 part Epoxy | Mixing Defoaming | ARE-250 20 seconds | Epoxy Part A: 3000-6000 poise Part B: 0.3-0.7 poise | View |
4 | Carbon Nano Fiber (10V%) | Dispersion | ARE-250 3 minutes | CNF-10 volume % Nano particle, Fiber | View |
5 | Carbon Black 2 part silicone (20 wt%) | Dispersion Defoaming | ARV-310 1 minutes/ ARE-250 8 minutes | Nano Carbon Black 20wt% (50V%) Nano particle (Total 120g) | View |
6 | Silicone Potting Compounds | Mixing Defoaming | ARV-310 3 minutes | Part A: 4000-8000 poise Part B: 200-700 poise (Total 10g) | View |
7 | Precious metal paste | Dispersion Defoaming | ARV-310 / ARE-250 from 30 sec. to 1 min | General silver filled condudctive epoxy / Jar and syringe application Highly dense metal powder | View |
8 | Carbon NanoTube (1-2 wt%) | Dispersion | ARV-310 6 min | CNT – 1-2 wt% Nano particle tube | View |
9 | Zinc Oxide(10 V%) | Dispersion Defoaming | ARE-250 6 min | ZnO 10 volume % petroleum Jelly 0.85, Zinc Oxide 5.76 | View |
10 | LCD ODF sealant (10V%) | Dispersion Deforming | ARV-5000 TWIN | Au Ball 10 volume % sealant 400,000cP, Au ball 3µ | View |
11 | Printing Ink | Degas | ARV-5000 | Solvent Ink 450g | View |
12 | Viscous Epoxy | Defoaming | ARE-250250AD-EFD-3×6 | Epoxy 828 2.5cc in EFD 3cc Syringe | View |
13 | Alumina | Dispersion Defoaming | ARV-5000 | Aluminum oxide – 20 volume % Silicone 3000cP | View |
14 | LED Phosphor | Dispersion Defoaming | ARV-310+ Syringe Loader | Phosphor 10 wt% Slicone 10,000cP 20g | View |
15 | Viscous Epoxy | Defoaming | ARV-310 + Syringe Loader | Various Epoxy sample | View |
16 | Talc | DispersionDefoaming | ARE-250 | Silicone 60g – 30wt% Silicone 10,000cP | View |
17 | CNF (1%wt) | Dispersion Defoaming | ARV-310 6min | CNF 1%wt | View |
18 | Suspension | Particle Reduction | ARE-250 3min | Phenytoin as API | View |